1بخش تحقیقات علوم چوب و فرآوردههای آن، مؤسسه تحقیقات جنگلها و مراتع کشور، سازمان تحقیقات، آموزش و ترویج کشاورزی، تهران، ایران
2گروه علوم و صنایع چوب و کاغذ، دانشگاه آزاد اسلامی واحد کرج
3موسسه تحقیقات جنگلها و مراتع . بخش تحقیقات علوم چوب و کاغذ صندوق پستی 116- 13185 تهران – ایران
4بخش تحقیقات علوم چوب و فرآوردههای آن، موسسه تحقیقات جنگلها و مراتع کشور
عنوان مقاله [English]
Investigation on potential long fibre Pinus eldarica Kraft Pulp
نویسندگان [English]
Fardad Golbabaei1؛ Ahmad Jahan latibari2؛ Abdolrahman Hosseinzadeh3؛ Sayed Javad Sepidehdam1؛ Amir Nourbakhsh4
1Wood and Forest Products Science Research Division, Research Institute of Forests and Rangelands,
Agricultural Research Education and Extension Organization (AREEO) P.O. Box 13185-116, Tehran, Iran
2Islamic Azad University, Karaj, Iran
3Wood and forest products division, Research Institute of Forests and Rangelands, Agricultural Resear
4Wood and Paper Science Research Division, Research Institute of Forests and Rangelands , Iran,
چکیده [English]
Kraft pulping of Pinus eldarica wood was carried out at 18% active alkali, 25% sulphidity and pulping temperature & Time of 165 C and 90 minutes pulp was compared with imported unbleached long fibre pulp with the kappa number of 34. Pinus eldarica pulp (500 ml csf) and imported long fibre pulp 120 g/m2 hand sheets were prepared for testing. Blending ratios were kept at 5, 10, 15 and 20% for both long fibre pulps.
Upon mixing 5, 10, 15, 20% Pinus eldarica pulp with hardwood pulp, breaking length increased to 6.9, 7.77, 8.01 and 9.14 Km. Respectively, and corresponding figures for imported pulp addition were 6.71, 8.2, 8.25 and 9.27 Km respectively. Tear index is also measured. Adding 5, 10, 15, 20% Pinus eldarica pulp to local hardwood pulp produced tear indexes of 5.93, 6.95, 6.65, 7.08 mNm2/g respectively and corresponding figures for imported pulp 5.38, 5.61 and 5.60 kPa. m2/g with blending above percentages of P. eldarica pulp and 4.78, 5.27, 5.38 and 6.23 kPa. m²/g upon addition of imported pulp.